CP-MP10 is organic modified bentonite clay. It can be used in low, medium and high polarity (ketones, ester, ether esters, alcohols, aromatic)systems.
Typical properties
Composition Organic derivative of a montmorillonite clay
Appearance Fine powder, light yellow
Moisture content (105 Degree,2hr) Max. 3.5%
Viscosity, mPa.s 3000-6000
Loss on ignition %(1000 Degree) 32-35
Bulk density 0.46-0.48 g/cm3
Fineness (