Provides high strength and heat resistance properties due to high aluminum content and silicon doping. The maximum operating temperature is 480 ° C The alloy is thermally stable, plastic, crack resistant. Double and isothermal annealing provides an optimal combination of properties; the β-phase content in the annealed alloy is about 10%.
Application: Mainly used in GTE details (discs, low pressure compressor blades, fan mounting parts).
State Standards 19807-91TU1-92-148-89
Chemical composition , %:
Ti -Prin
Al - 5.8-7.0
Mo -2,8-3,8
Zr -0,50
Si-0.2-0.4
Fe -0,30
O2 -0.15
H2 -0,015
N2 -0.05
C -0,10
Mixtures -0.30